Abstract
Deep tissue imaging requires the combination of long wavelength excitation and emission to avoid absorption by tissue in vivo. Theranostics, which combines imaging and therapeutic drug delivery, will also be aided by being able to image deeply in vivo. We present a new nanoparticle construct that enables long-wavelength imaging, and encapsulation of therapeutics. It is based on the ability of Flash NanoPrecipitation (FNP) to assemble hydrophobic inorganic and organic species in a single precipitation step. The NPs are based on 72 nm diameter upconverting phosphors (UCPs) that are excited at 980 nm and emit at shorter wavelengths. The UCPs are coated in the precipitation step with a layer of fluorescent dye, DiR, that is excited at the emission wavelength of the UCP. However, the shorter wavelength excitation of the UCP is transferred by Förster energy transfer rather than radiative excitation. The DiR on the UCP surface strongly emits with a maximum at 780 nm. These upconverting nanoparticles (UCNPs) have three distinctive advantages: The UCPs excitation, at 978 nm, is driven by high power, inexpensive laser diodes used for fiber optic communications. Second, the large wavelength difference between excitation (980 nm) and emission (780 nm) reduces the problem of blocking filters that are required when the adsorption and emission spectra closely overlap. Third, both excitation and emission wavelength are in the “imaging window” with minimal absorption from tissue, blood, or water. These advantages make this an attractive platform for developing theranostic NPs. The incorporation of therapeutic compounds into this upconverting nanoparticle (UCNP) platform is presented.
Keywords:
UCP
; up converting phosphors
; DiR
; theranostics
; nanoparticles
; FNP
; flash nanoprecipitation
; Forester energy transfer
; FRET
1. Introduction
Current deep tissue imaging is done using long wavelength dyes. To achieve long wavelength emission large organic molecules that can support electron resonance are used. They are driven into an excited state by high energy photons and emit lower energy (longer wavelength) photons. There are some intrinsic limitations in the field of bioimaging: (1) The photon absorbance in tissue provides a “window” in which adsorption (of the exciting or emitted photon) is minimum between about 650 nm and 1.3 microns as shown in Figure 1 [1]. Dyes with shorter wavelength excitation are too strongly absorbed to enable deep tissue imaging. Dyes with emissions above 850 nm require cooled and more expensive detectors that limits their wide adoption [2]. In most applications, to increase the measured fluorescence signal the excitation wavelength is set close to the emission peak (20–30 nm bandwidth filters). At high illumination intensities, this challenges the precision of the filters, and a significant fraction of emitted, longer wavelength photons are blocked by the filters in the detector train. This is illustrated in Figure 2 which is the absorption and emission spectra for DiR dye: the absorption maxima is 745 nm and the emission maxima is 780 nm.
Our strategy is to use the upconverting phosphor (UCP) nanocrystals as the core of a nanoparticle (NP) to make an upconverting nanoparticle (UCNP). The UCPs absorb photons at 978 nm and emit at shorter, higher energy wavelengths. By coating the UCP crystal with a hydrophobic fluorescent dye, the UCP excited state energy can be transferred to the fluorescent dye and its emission to the ground state occurs at longer wavelengths charactristic of that dye. Importantly, the fluorescence at longer wavelength is still in the imaging window of ~800nm.
The technological advance that make this UCP nanoparticle interesting as an imaging particle is the development of solidstate laser diodes that emit at 978nm. This is the basis of commercial optical fiber technology because at this wavelength there is essentially no absorption due to water or hydroxyls, thus enabling long distance fiber optic transmission. Multi-watt laser diodes coupled to fiber optic cables are inexpensive. We used a Thorlabs F240FCB collimated Qphotonics 978 nm diode laser, driven with a Thorlabs LDC3065-488 High-Power Laser Diode Driver (Thorlabs, Newton, New Jersey). the optical fiber excitation was focused on the cuvette in a Hitachi F-7000 fluorometer (Hitachi High-Technologies Science America, 19865 Nordhoff St., Northridge, CA.). Emission was monitored at 90.o . The UCNPs have also been used in a fluoresence microscope system illuminated by the 978 nm laser diode, and the laser diode could adapted to whole animal imaging instruments.
The research objectives are the selection of the dye, how to efficiently coat the UCPs with the fluorescent dye and determination of the most effective coating thickness.
2. Materials and Methods
UCNPs are sodium yttrium fluoride (NaYF4) nanocrystals doped with lanthanides which can convert two or more near-infrared (NIR) photons to one visible photon by sequential electronic excitation and energy transfer processes [3]. The emission spectra of UCNPs can be tuned by manipulating the lanthanide doping. Specifically, NaYF4: Er3+/Yb3+ UNCPs are green emitting while NaYF4: Tm3+/Yb3+ are blue emitting [4]. UCNPs are synthesized by cothermolysis of trifluoroacetate precursors with coordinating ligands in order to control particle size [3]. The following coordinating ligands have been shown to be effective in producing monodisperse and size-tunable UCNPs with hydrophobic surfaces: Oleic acid (OA), oleyl amine (OM), trioctylphosphine (TOP), trioctylphosphine oxide (TOPO), and OA-TOP [3]. The OA-TOP coordinating ligand is the most effective at producing bright B-phase (hexagonal crystals) UCNPs [3]. UCNPs are resistant to photobleaching, have low toxicity, do not exhibit significant autofluorescence, have narrow absorption and emission spectra, and show high quantum yield [5]. UCNPs used here are synthesized using the high temperature cothermalysis method described by Shan, et al. [3,5]. Figure 3 shows a transmission electron microscopy (TEM) image of UCNPs. If UCPs are doped with Yb3+/Er3+, there are two major emission peaks: 560 nm and 650 nm (Figure 3). The shorter wavelength emissions of the UCPs would be outside the “imaging window” and subject to signal loss. Therefore, we developed a coating strategy to coat the UCP with a fluorophore that will transfer the excited UCP energy to the coating dye, which will then emit a longer wavelength photon. This shifts the photons from the UCNP from short wavelength to longer wavelength, which is in the imaging “window”.
The energy transfer is not a traditional radiative energy excitation process, but rather a Förster Resonance Energy Transfer or Fluorescence Resonance Energy Transfer (FRET) emission. FRET emission occurs when the distance between the UCP and the fluorophore is less than the wavelength of the photon that would typically be emitted by the UCNP [6]. Instead, the acceptor fluorophore absorbs energy from the donor UCNP in its excited state and emits this energy as a photon; it does not absorb a photon from the UCNP [12]. FRET emission can only occur between a donor and an acceptor fluorophore whose emission and excitation peaks, respectively, overlap and where the distance between the donor and the acceptor is withing the Förster distance, which is typically 20–90 nm [6]. FRET excitation and emission is controlled by dipole-dipole interactions between the donor and the acceptor fluorophores [12]. The FRET energy transfer rate is proportional to the inverse sixth power of the distance between the fluorophores 6:
Eq.1
where is the rate of energy transfer from donor to acceptor
is the radiative decay of the donor fluorophore (inverse of the fluorescence emission lifetime in the absence of the acceptor, typically 1-50 ns), r is the distance between the two molecules, and is the Förster distance (characterized by the 50% efficiency point of the energy transfer, typically 20–90A). It is possible to dope UCP crystals with Yb and Tm to obtain direct excitation at 800 nm. However, the FRET emission pathway is an order of magnitude more efficient in producing emitted photons.
The fluorescent emission dye was coated on the UCP crystals using Flash NanoPrecipitation (FNP) [7,8]. The requirements for the coating dye are that it has sufficient hydrophobicity to remain on the UCP surface, that its absorption matched the UCP emission wavelengths and that its emission was in the desire wavelength range. Several dyes were considered, the dye chosen was 1,1’-dioctadecyl-3,3,3’,3’-tetramethylindotricarbocyanine iodide (DiR). Its adsorption and emission spectra are shown in Figure 2.
The spectra show that there is minimal adsorption of the 980 nm excitation illumination; therefore, the dye coating will not cause attenuation of the excitation illumination. Also, the excitation spectrum shows that the 650-emission peak of the UCP matches the adsorption shoulder on the DiR dye. The large wavelength differences between the 980 nm excitation wavelength, the 650 nm UCP emission and the DiR emission maxima at 780 make the problem of optical filter bleed-through less problematic. Also, the 130 nm wavelength difference between the UCP emission and the DiR adsorption peak means that a broad range of wavelengths of the emission spectra can be collected to provide bright immaging.
The UCPs were synthesized, as described earlier [9], by high temperature decomposition of the TOPA chelate to provide nanocrystals with uniform size and hydrophobic surfaces.
The coating was applied using the Flash NanoPrecipitation (FNP) process. This is rapid precipitation process using turbulence to mix solvent and antisolvent streams to produce high supersaturations in ~1.5 ms. The FNP process has been used to produce NPs from hydrophobic small molecule drugs, from peptides and proteins, and from nucleic acids. The COVID vaccines are produced by this process. It has also been used to encapsulate and coat inorganic colloids and particles. Wilson [10,11] has presented the “rules” for the incorporation of inorganic core particles into coated NPs. Because of differences in diffusion times and distances, when larger core colloids are coated, a population of polymeric micelles that do not contain the inorganic core are produced. The coated NPs are easily purified; micelles are easily removed by centrifugation and decanting.
UCP crystals were dispersed in THF solvent with DiR and a stabilizing block copolymer (polystyrene-b-polyethylene glycol (PS-PEG) with molecular weights 1.5K- 5K Da). A constant UCNP concentration of 1 mg/mL was used. A four-jet Multi Inlet Vortex Mixer (MIVM) [12,13] was used with one organic stream flowrate at 12 mL/min and the three aqueous streams each at 12 mL/min. These flowrates were selected in order to obtain an appropriate Reynolds number within the micromixer. The UCNPs were dialyzed against nanopure water over 24 hours using cellulose tubing (Spectra/Por, MWCO 12-14K), changing the water at least three times. The suspension was then centrifuged at 14,000 RPM for 30 min. (Eppendorph Centrifuge 5430 R) to remove empty micelles and to concentrate the samples.
Dynamic light scattering (DLS) (Malvern Instruments) measurements were taken immediately after micromixing, after dialysis, and after centrifugation in order to measure particle size distribution. DLS was also used to confirm that empty micelles were removed via centrifugation. DLS was performed by taking a 100 uL sample diluting it with 900 uL of nanopure water in a DLS cuvette.
The fluorescence upon 980 nm excitation was measured using a NIR diode laser (Thor Labs,) illuminating the sample in a Hitachi F-7000 fluoromoter.
3. Results
UCNP were made at a fixed concentration of UCPs of 1 mg/mL with variable DiR concentrations of: 1 mg/ml, 0.5 mg/mL, 0.2 mg/mL, 0.1 mg/mL, 0.02 mg/mL, and 0.01 mg/mL. The compositions are shown in Table 1.
The coating thickness on the 72 nm crystals are estimated to be 26 nm for the highest concentration of DiR, 1 mg/mL. This estimate is somewhat high because DiR that was captured in micelles, and remove by decanting, would reduce the amount of DiR that actually coats the UCP. At the DiR concentration of 0.1 mg/mL the coating thickness would be 8.6 nm, and at 0.01 mg/mL the coating would be 0.5 nm. The coating has two effects. First, it adsorbs the emitted fluorescence since the absorption and emission spectra strongly overlap. Second, the dominant fluoresence emission comes from the Förster energy transfer from the crystal to the encapsulating DiR shell. The typical Forester energy transfer distance is 0.2–0.9 nm. Therefore, much of the DiR in the shell for the 1 mg/mL loading (thickness = 26 nm) would be beyond this energy transfer distance, and the fluorescence emission would be less efficient, and the emitted fluorescence would be adsorbed within the thick layer.
The results of the coating concentration on the fluorescence measurements on the dispersions are shown in Figure 4. There is a strong maximum. At 0.04 mg/mL DiR the fluorescence is 1700 AU. Whereas at the higher loading of 0.5 mg/mL the fluorescence intensity drops to less than 100 AU The maximum fluorescence intensity is when the coating thickness is approximately equal to the Förster energy transfer distance. This thickness allows maximal energy transfer between the cyrstal and the DiR coating and minimizes fluorescence absorbance by DiR in the layer.
Theracostic application
At this stage we have demonstrated the assembly of a novel fluorescent nanocarrier that uses high power laser light at 980nm to enable deep tissue pepentration. The UCP upconverts this to a shorter wavelength emission at 615 nm and 650 nm. The 650 nm emission has strong overlap with the shoulder adsorption band of DiR and causes emission that has its maximum emission at 780 nm. An important point is that the excitation at 980 nm and the emission at 789 nm are beam are within the optical window that minimizes attenuation in tissue applications. If the direct UCP emission at 650 nm was used for imaging it would be attenuated by 80% relative to the 789 nm emission. Theranostic means that a nanoparticle delivers both a therepeutic and a diagnostic function. Here we have emphasized the diagnostic (imagine) capabilities of these particles. However, earlier we demonstrated that hydrophobic therapeutic agents can be co-encapsulated with ionorganic colloids. We demonstrated the co-encapsulation of meso -tetraphenyl porphine (TPP), which acts as an oxygen radical initiator for photodynamic therapy with UCP crysals [3]. Organic polymers of a wide range of molecular weight have been co-encapsulated with iron oxide magnetic particles [5,10]. The FNP process enables co-encapsulation of multiple species. D’Addio demonstrated that multiple hydrophobic drugs could be encapsulated into NPs by FNP [14]. Pinkerton showed that inorganic colloids, drugs and hydrophobic dyes could be encapsulated by FNP [15]. Therefore the extension of adding a therapeutic drug to the UCP and DiR composition is straightforward.
References
- Pansare, V. J.; Hejazi, S.; Faenza, W. J.; Prud’homme, R. K. Review of long-wavelength optical and NIR imaging materials: contrast agents, fluorophores, and multifunctional nano carriers. Chem. Mater. 2012, 24(5), 812–827. [Google Scholar] [CrossRef] [PubMed]
- Boulnois, J.-L. Photophysical processes in recent medical laser developments: a review. Lasers Med. Sci. 1986, 1(1), 47–66. [Google Scholar] [CrossRef]
- Budijono, S. J.; Shan, J.; Yao, N.; Miura, Y.; Hoye, T.; Austin, R. H.; Ju, Y.; Prud’homme, R. K. Synthesis of stable block-copolymer-protected NaYF4: Yb3+, Er3+ up-converting phosphor nanoparticles. Chem. Mater. 2010, 22(2), 311–318. [Google Scholar]
- Kulak, A.; Hall, S. R.; Mann, S. Single-step fabrication of drug-encapsulated inorganic microspheres with complex form by sonication-induced nanoparticle assembly. Chem. Commun. 2004, 40(5), 576–577. [Google Scholar] [CrossRef] [PubMed]
- Shan, J.; Ju, Y. A single-step synthesis and the kinetic mechanism for monodisperse and hexagonal-phase NaYF4: Yb, Er upconversion nanophosphors. Nanotechnology 2009, 20(27), 275603. [Google Scholar] [CrossRef] [PubMed]
- Gabor, M. the Use of Fluorescence in Research Into Protein Structures. [CrossRef] [PubMed]
- D’Addio, S. M.; Prud’homme, R. K. Controlling drug nanoparticle formation by rapid precipitation. Adv. Drug Deliv. Rev. 2011, 63(6), 417–426. [Google Scholar] [CrossRef] [PubMed]
- Saad, W. S.; Prud’homme, R. K. Principles of nanoparticle formation by flash nanoprecipitation. Nano Today 2016, 11(2), 212–227. [Google Scholar] [CrossRef]
- Shan, J.; Budijono, S. J.; Hu, G.; Yao, N.; Kang, Y.; Ju, Y.; Prud’homme, R. K. Pegylated composite nanoparticles containing upconverting phosphors and meso-tetraphenyl porphine (TPP) for Photodynamic Therapy. Adv. Funct. Mater. 2011, 21(13), 2488–2495. [Google Scholar] [CrossRef]
- Wilson, B. K.; Prud’homme, R. K. Co-encapsulation of organic polymers and inorganic superparamagnetic iron oxide colloidal crystals requires matched diffusion time scales. Soft Matter 2024, 20(41), 8312–8325. [Google Scholar] [CrossRef] [PubMed]
- Wilson, B. K.; Prud’homme, R. K. Nanoparticle size distribution quantification from transmission electron microscopy (TEM) of ruthenium tetroxide stained polymeric nanoparticles. J. Colloid Interface Sci. 2021, 604, 208–220. [Google Scholar] [CrossRef] [PubMed]
- Liu, Y.; Cheng, C.; Prud’homme, R. K.; Fox, R. O. Mixing in a multi-inlet vortex mixer (MIVM) for flash nano-precipitation. Chem. Eng. Sci. 2008, 63(11), 2829–2842. [Google Scholar] [CrossRef]
- Markwalter, C. E.; Prud’homme, R. K. Design of a small-scale multi-inlet vortex mixer for scalable nanoparticle production and application to the encapsulation of biologics by inverse flash nanoprecipitation. J. Pharm. Sci. 2018, 107(9), 2465–2471. [Google Scholar] [CrossRef] [PubMed]
- D’Addio, S. M.; Reddy, V. M.; Liu, Y.; Sinko, P. J.; Einck, L.; Prud’homme, R. K. Antitubercular nanocarrier combination therapy: Formulation strategies and in vitro efficacy for rifampicin and SQ641. Mol. Pharm. 2015, 12(5), 1554. [Google Scholar] [CrossRef] [PubMed]
- Pinkerton, N. M.; Gindy, M. E.; Calero-DdelC, V. L.; Wolfson, T.; Pagels, R. F.; Adler, D.; Gao, D.; Li, S.; Wang, R.; Zevon, M. Single-Step Assembly of Multimodal Imaging Nanocarriers: MRI and Long-Wavelength Fluorescence Imaging. Adv. Healthc. Mater. 2015, 4(9), 1376–1385. [Google Scholar] [CrossRef] [PubMed]
Figure 1.
Absorption spectra of water, protein, melanin, oxidized hemoglobin (Hb02), hemoglobin (Hb), and collagen. These spectra illustrate the narrow window for fluorescent excitation and emission that does not result in significant losses to photon absorption by components commonly present in biological systems (from ref 2).
Figure 1.
Absorption spectra of water, protein, melanin, oxidized hemoglobin (Hb02), hemoglobin (Hb), and collagen. These spectra illustrate the narrow window for fluorescent excitation and emission that does not result in significant losses to photon absorption by components commonly present in biological systems (from ref 2).

Figure 2.
DiR excitation and emission spectra. DiR’s excitation peak is at 740 nm and its emission peak is at 780 nm. [Invitrogen emission and excitaion spectra www.invitrogen.com].
Figure 2.
DiR excitation and emission spectra. DiR’s excitation peak is at 740 nm and its emission peak is at 780 nm. [Invitrogen emission and excitaion spectra www.invitrogen.com].

Figure 3.
TEM of UCP crystals using high temperature thermolysis method with OA-TOP chelating ligand. Emission spectra of UCPs upon excitation with 978 nm laser illumination.
Figure 3.
TEM of UCP crystals using high temperature thermolysis method with OA-TOP chelating ligand. Emission spectra of UCPs upon excitation with 978 nm laser illumination.

Figure 4.
Peak fluorescence intensity (on 980 nm NIR laser excitation) on DiR concentration is shown on the left and full fluorescence spectra for the serial dilution series of DiR in THF is shown on the right. The fluorescence peak goes through a maximum at approximately 0.04 mg/mL DiR in THF due to the quenching effect.
Figure 4.
Peak fluorescence intensity (on 980 nm NIR laser excitation) on DiR concentration is shown on the left and full fluorescence spectra for the serial dilution series of DiR in THF is shown on the right. The fluorescence peak goes through a maximum at approximately 0.04 mg/mL DiR in THF due to the quenching effect.

Table 1.
UCNP-DiR NP formulations. The first column denotes the experiment reference number. The second column is the reference number for the UCNP batch number. The leading letter in the third column references the diblock copolymer used, PS-PEG (1.5K-5K) and the ratio is the mass ratio of UCNPs to polymer. The fourth column shows the masses of UCNPs, DiR, and THF in the organic stream of each formulation. The UCNP to DiR mass ratios for Experiments 51-56 are1:1, 2:1, 5:1, 10:1, 50:1 and 100:1, respectively. The compositions are designed to reveal the effect of diluting the DiR in the NP core by increasing the ratio of UCNP to DiR.
Table 1.
UCNP-DiR NP formulations. The first column denotes the experiment reference number. The second column is the reference number for the UCNP batch number. The leading letter in the third column references the diblock copolymer used, PS-PEG (1.5K-5K) and the ratio is the mass ratio of UCNPs to polymer. The fourth column shows the masses of UCNPs, DiR, and THF in the organic stream of each formulation. The UCNP to DiR mass ratios for Experiments 51-56 are1:1, 2:1, 5:1, 10:1, 50:1 and 100:1, respectively. The compositions are designed to reveal the effect of diluting the DiR in the NP core by increasing the ratio of UCNP to DiR.
| NCT Number | Intervention |
| NCT06176729 | Polatuzumab vedotin + rituximab + lenalidomide |
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content. |
© 2026 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license.
Copyright: This open access article is published under a Creative Commons CC BY 4.0 license, which permit the free download, distribution, and reuse, provided that the author and preprint are cited in any reuse.